Chengdu Daguang New Materials | COT800 Cobalt-Based High-Temperature Wear-Resistant
COT800: A Cobalt-Based Wear-Resistant Alloy That Does Not Rely on Carbides, Designed for High-Temperature, Unlubricated Service
Getting to Know COT800
|
Element |
Co |
Mo |
Cr |
Si |
C |
Ni, Fe |
|---|---|---|---|---|---|---|
|
Content |
Balance |
27–30% |
16.5–18.5% |
3.0–3.8% |
≤0.08% |
≤3% |
Corresponding grades: Tribaloy T-800, UNS R30800. Hardness 54–62 HRC, density approx. 8.6 g/cm³, melting point 1288–1352°C.
01 First, the Answer: The Cobalt-Based Odd One That Does Not Take the Carbide Route
The Tribaloy series is designed on a completely different principle from Stellite. Stellite relies on carbides; Tribaloy relies on an intermetallic Laves phase (a cobalt–molybdenum–silicon compound). The Laves phase makes up more than 50%, has a melting point around 1560°C—higher than the alloy itself—and is dispersed in a cobalt-based eutectic matrix. It is like planting a batch of crystals in the metal that are harder and more heat-resistant than the matrix: wear hits them first, while the matrix bears the impact and keeps the structure from fracturing.
02 Why Being Oil-Free Actually Works Better: Self-Lubrication Plus High Cr and Mo
Among the cobalt-based series, COT800 has the highest molybdenum content (about 28%), and this is the confidence behind its ability to handle dry friction: at high temperature, molybdenum oxides form a lubricating film on the rubbing surfaces. Under oil-starved, oil-cutoff or boundary-lubrication conditions, it does not seize against the mating part—the friction coefficient is low and galling resistance is strong. Meanwhile, the high chromium and molybdenum give it excellent oxidation resistance and corrosion resistance, with service temperatures reaching on the order of 900–1000°C in specific environments. In one sentence: other alloys rely on oil; it relies on its own composition.
03 One Table to See the Difference Between COT800 and Carbide-Based Cobalt Alloys
|
Comparison |
COT800 |
CO6 |
CO1 |
|---|---|---|---|
|
Strengthening phase |
Laves-phase intermetallic |
Carbides |
Carbides |
|
Carbon content |
≤0.08% |
~1% |
2.0–3.0% |
|
Hardness |
54–62 HRC |
~40 HRC |
50–58 HRC |
|
Unlubricated friction |
Excellent |
Fair |
Fair |
|
High-temperature service |
On the order of ~1000°C |
~500°C |
760°C+ |
|
Galling resistance |
Outstanding |
Good |
Good |
|
Typical applications |
Dry-friction seal faces |
General wear resistance |
Extreme wear |
The core difference of this table is one sentence: carbide-based cobalt alloys compete on abrasives and erosion, while COT800 competes on dry friction and galling resistance at high temperature. They are not substitutes but a division of labor.
04 Which Components Call Out COT800
Mechanical seal rotating and stationary rings, pump seal faces. Oil cutoff, dry running, high temperature—COT800 is the specialist for such seal faces.
Turbochargers, automotive valve seats and guides. High-temperature reciprocating friction; it must not seize even when briefly oil-starved.
Galvanizing-roll bushings, cams, retaining rings. High-temperature roll-face friction; the Laves phase’s heat and wear resistance are put to use.
Aircraft-engine wearing surfaces, valve seal faces, bearing seats, diesel piston rings. All are typical scenarios of high temperature plus possible oil starvation.
Turbochargers run at high temperature and high speed; locally oil-starved conditions are exactly where COT800 earns its keep.
05 Three Reminders for Using COT800
1. Preheat for surfacing. The Laves phase is brittle; for PTA surfacing or laser cladding, preheat to 500–650°C and cool slowly after welding to prevent cracking.
2. Machining by grinding and EDM only. At 54–62 HRC plus the Laves phase, carbide cutting tools can hardly bite; downstream machining uses EDM or grinding with diamond/silicon carbide.
3. Do not use it as a carbide-based cobalt alloy. For pure abrasive-wear service, CO1 and CO20 are more direct; COT800’s value lies in high temperature plus no lubrication plus galling resistance—match the selection to the service.
06 How Peers Map to It (All Correspond to COT800)
|
Manufacturer |
Grade |
|---|---|
|
Chengdu Daguang New Materials |
COT800 |
|
Kennametal Stellite (original) |
Tribaloy T-800 |
|
Oerlikon Metco |
Diamalloy 3001, Metco 68F-NS-1 |
|
Höganäs |
AMPERIT 342 |
|
FST |
M-499 |
Back to Selection: Remember Three Sentences
High temperature, oil-starved, afraid of seizing? Use COT800.
Preheat 500–650°C before surfacing, and prepare EDM and diamond grinding for machining.
Carbide-based cobalt alloys compete on wear; COT800 competes on unlubricated service.
Chengdu Daguang New Materials · Material Science Series
What to know about this product?
SEND A MESSAGE
Something isn't Clear?
Feel free to contact me, and l will be morethan happy to answer all of your questions.